It is prepared by ultra-high molecular weight polyethylene polymerization process, and after micronization treatment, the particle size is only 5-10μm, which can be evenly dispersed in the powder coating system without agglomeration. Its ultra-low friction coefficient can effectively reduce the wear rate of the coating surface, improving the scratch resistance of the coating, without destroying the original adhesion and gloss of the coating. It passes strict ROHS 2.0 compliance testing, does not contain heavy metals and harmful volatile substances, adapting to global environmental protection coating standards.

Melting Point: 130-140℃, Weight Average Molecular Weight: 3000-5000, Friction Coefficient (steel to steel): 0.12-0.15, Density (25℃): 0.97-0.99 g/cm³, Appearance: White ultra-fine powder, Average Particle Size: 5-10μm, Volatile Matter (105℃, 2h): ≤0.2%, Closed Flash Point: 280℃, Acid Value: ≤0.3 mgKOH/g, Water Content: ≤0.05%, Thermal Decomposition Temperature: ≥320℃.

It is mainly used in formula modification of thermosetting powder coatings and thermoplastic powder coatings, including home appliance shell coating, auto parts primer coating, outdoor metal furniture coating, fitness equipment protective coating and other scenarios. It can be added to powder coating systems as a slip agent, wear-resistant agent and release agent, helping manufacturers improve the appearance quality and protective performance of the coating. It is compatible with all types of powder coating production equipment and coating processes, suitable for powder coating production enterprises of all scales, supporting the development of high-performance protective coatings.